MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex APEX® 80853-C Nat 14 Polyvinyl Chloride, Flexible
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade; PVC, Wire and Cable Grade

Material Notes: Notes: 105°C, Non-lead Stabilized, Insulation; PVC Insulation intended for use in 90°C wet locations; RoHS Compliant

Features: Flame Retardant; Oil Resistant

Uses: Insulation; Wet Rated Insulation; Wire and Cable Applications

Agency Ratings: UL I Oil Rating; UL QMTT2 .E73402

Forms: Pellets

Wire Types: MTW; THW-2; TW; THHN; THWN; THW; THWN-2

Information Provided by Teknor Apex

Key Words: PVC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore C 7310 seconds; ASTM D2240
Tensile Strength at Break 3100 psiASTM D638
Elongation at Break 350 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.40e+15 ohm-cmASTM D257
Dielectric Constant 2.99
@Frequency 1e+6 Hz
ASTM D150
 4.36
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 880 V/milASTM D149
Dissipation Factor 0.058
@Frequency 1e+6 Hz
ASTM D150
 0.095
@Frequency 1000 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 221 °FContinuous Use; ASTM D794
Brittleness Temperature -2.20 °FASTM D746
Oxygen Index 29 %ASTM D2863
 
Descriptive Properties
AppearanceOpaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AlphaGary Garaflex™ E 4771-A8 OR1 LCF Vinyl Thermoplastic Elastomer
Teknor Apex APEX® 84842 Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80853-B Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80853-A Polyvinyl Chloride, Flexible
Teknor Apex APEX® 80851-F Polyvinyl Chloride, Flexible

PTEKNO475 / 128652

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.