MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sinotek Materials Packing Carbonized Fiber Braided
Categories: Carbon; Carbon Fiber/Carbon Fibre

Material Notes: The packing is manufactured in the following procedures: polyacrylonitrile fiber is heated into carbonized fiber, which is woven into packing after impregnation in PTFE dispersion containing graphite particles. It is used as dynamic sealing in the presence of media of weak acid or alkaline, or media that contain few grains of solid particles.

Information provided by Sinotek

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 2.0 - 12
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 260 °C
 
Descriptive Properties
Max Working Pressure, MPa10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sinotek Materials Packing Carbon Fiber with Graphite
Zoltek™ PX35 UD150 Uni-Directional Carbon Fabric
Carlisle 201LD Carbon-Carbon Composite
Hexcel® HexTow® AS4C 3K Standard Modulus Carbon Fiber (3000 Filaments)
DowAksa AKSACA™ A-38 3K Continuous Carbon Fiber

CSINOT74 / 2131

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.