MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polynt DISTITRON® 161 T100Z Unsaturated Polyester Resin
Categories: Polymer; Thermoset; Polyester, TS

Material Notes: Unsaturated polyester resin in styrene, Orthophthalic

Appearance: Neutral – Opalescent

Main resin characteristics: Thixotropic, With antifoaming additive

Main applications: Buttons

Molding information: Casting (rods)

Curing cycle: 24h at 23°C + 2h at 100°C + 1h at 100°C

Information provided by Polynt Composites.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.10 g/cc0.0397 lb/in³
Solids Content 67 - 71 %67 - 71 %MT-CU001C
Brookfield Viscosity 2900 - 3600 cP2900 - 3600 cPsp 3 rpm 20; MT-CUT23V
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 2929ASTM D 2583
Tensile Strength 35.0 MPa5080 psiISO 527
Elongation at Break 13 %13 %ISO 527
Tensile Modulus 2.00 GPa290 ksiISO 527
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 42.0 °C108 °FISO 75 -2A
 
Processing PropertiesMetricEnglishComments
Gel Time 19.0 - 24.0 min
@Temperature 20.0 °C
19.0 - 24.0 min
@Temperature 68.0 °F
Reactivity at 20°C + 0,4% Co 1% + 2% MEKP50; RS.08.G
Shelf Life 3.00 Month3.00 Monthin the dark; MT-CU002S
 
Descriptive Properties
Peak Exotherm135 - 165°CRS.08.G; Reactivity at 20°C + 0,4% Co 1% + 2% MEKP50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOLYN9382 / 231977

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.