MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Hifax 5519/1 G 1750 Polypropylene, 10% Talc Filled  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 10% Talc Filler

Material Notes: Hifax polypropylene resins based on the Catalloy process are used in applications such as building and construction, industrial applications, and also automotive industries. Hifax provide customers with good processability, excellent impact resistance, a broad range of stiffness from very soft to rigid products, high temperature resistance and low linear coefficient of thermal expansion.

Hifax 5519/1 G 1750 is a less then 10% talc filled PP copolymer, with good impact resistance. Product is available as a customized color matched, pellet form. This grade is delivered in 1750 color version. Applications: Bumpers.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.970 g/ccISO 1183-1/A
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17.0 MPaISO 527-1,-2
Elongation at Break 100 %ISO 527-1,-2
Flexural Modulus 1250 MPaTech.A; ISO 178/A1
Charpy Impact, Notched 6.20 kJ/m²
@Temperature -30.0 °C
ISO 179-1/1Ea
 60.0 kJ/m²
@Temperature 23.0 °C
ISO 179-1/1Ea
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 47.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 125 °CA50; ISO 306
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Buckeye Polymers BP RPP 1012 T BLK Polypropylene, Talc Filled
Clariant Renol PPT10 Polypropylene Copolymer, Talc Filled

PEQT7138 / 218775

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.