MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ IM7 12K Carbon Unitape
Categories: Polymer; Thermoset; Carbon Fiber/Thermoset Composite; Filled/Reinforced Thermoset

Material Notes: MVK-14 polyimide prepregs are a more affordable and easier-to-process, non-carcinogenic alternative to PMR-15 and other older polyimide chemistries. MVK-14 offers a more durable alternative to high-temp BMI’s, titanium and specialty metals. MVK-14 polyimide composites exhibit excellent mechanical and thermal properties in aerospace propulsion and airframe structure applications up to 600°F. MVK-14 is further supported by an FAA-conformed B-Basis Design-Allowable Database.

MVK-14 Polyimide materials can be processed using autoclave or compression-molding.

The product is available in fabric and unidirectional tape prepreg form, using carbon, quartz, ceramic and glass fibers.

Typical Properties: Autoclave cured at 600°F with 625°F air post cure.

Information provided by Renegade Materials Corporation.

Renegade Materials has been acquired by Teijin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles 10.5 - 13.5 %
Oxidative Stability 50 hour
@Temperature 316 °C,
Pressure 0.414 MPa
<2% wt loss
Thickness 5.50 milTypical, Cured Ply
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 143 ksi
@Temperature 21.1 °C
Test at RT after Oxidative Stability Test (600°F, 150 psia, 121 hrs)
 149 ksi
@Temperature 21.1 °C
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 490 °FWet, Storage Modulus
 643 °FDry, Storage Modulus
 
Descriptive Properties
Areal Fiber Weight140-150 gsmTypical
Prepreg Resin Content Range34-38%Typical
Void Content<3%Typical

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ T650-35 8HS Carbon Fabric
Solvay CYCOM® 5250-4 BMI Prepreg System with IM-7 Carbon Fiber
Solvay CYCOM® 2040 Epoxy Prepreg Fabric with 6KM46J-2X2T-200
Renegade Materials Corporation MVK-14 Polyimide FreeForm™ Astroquartz 4581 Fabric
Hexcel® HexTow® IM7 12K Intermediate Modulus Carbon Fiber (12,000 Filaments)

PRENEG07 / 138462

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.