MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Addiplast Addinyl A2I V25 Flame Retardant Nylon 66, 25% Glass Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Glass Fiber Filled, Flame Retardant

Material Notes: Flame retardant, 25% glass fiber reinforced, halogen free

Information provided by Addiplast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8989Conditioned; ISO 868
 9090ISO 868
Tensile Strength at Break 90.0 MPa13100 psiConditioned; ISO R 527
 130 MPa18900 psiISO R 527
Elongation at Break 5.0 %5.0 %ISO R 527
 6.0 %6.0 %Conditioned; ISO R 527
Modulus of Elasticity 5.50 GPa798 ksiConditioned; ISO 178
 7.80 GPa1130 ksiISO 178
Izod Impact, Notched (ISO) 8.50 kJ/m²4.04 ft-lb/in²ISO 180/1A
 9.50 kJ/m²4.52 ft-lb/in²Conditioned; ISO 180/1A
Charpy Impact Unnotched 6.00 J/cm²28.6 ft-lb/in²ISO 179/IeU
 6.00 J/cm²28.6 ft-lb/in²Conditioned; ISO 179/IeU
Charpy Impact, Notched 0.850 J/cm²4.04 ft-lb/in²ISO 179/IeA
 1.00 J/cm²4.76 ft-lb/in²Conditioned; ISO 179/IeA
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index >= 600 V>= 600 VCEI 60112/Solution A
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 3146/C2
Deflection Temperature at 1.8 MPa (264 psi) 245 °C473 °FISO 75-2/AF
Flammability, UL94 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
Oxygen Index 32 %32 %ISO 4589
Glow Wire Test 960 °C1760 °FCEI 60695/2/1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFADD926 / 156140

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.