MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

AMS 5315D(94) Ductile Iron
Categories: Metal; Ferrous Metal; Cast Iron; Ductile Iron

Material Notes: This specification is obsolete.

Key Words: 5315
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell <= 190<= 190
Tensile Strength, Ultimate 415 MPa60200 psi
Tensile Strength, Yield 310 MPa45000 psi
Elongation at Break 10 %10 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 3.2 - 4.0 %3.2 - 4.0 %
Iron, Fe >= 92.62 %>= 92.62 %As remainder
Manganese, Mn <= 0.80 %<= 0.80 %
Phosphorus, P <= 0.080 %<= 0.080 %
Silicon, Si 1.7 - 2.5 %1.7 - 2.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ductile Iron grade 60-40-18
Ductile Iron grade 80-60-03
High Silicon Ductile Iron at RT 4Si-0.9V nominal alloy content
Overview of materials for Ductile Iron
UNS F33101 Cast Iron

MWAMS5315 / 14298

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.