MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

solder replacement adhesives

(Viewing data as-entered. Click here to return)
Superior Flux Superior AL261-Series Direct Aluminum Solder Paste
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
  • Solders directly to aluminum for aluminum to copper and aluminum to aluminum connections
  • Eliminating the need for plating aluminum before soldering
  • Good thermal stability for heat sink reflow soldering
Description: Superior Solder Paste AL26-SERIES is a water-soluble formulation designed for direct aluminum to copper soldering of heat sinks. It also has excellent soldering characteristics for copper and nickel-plated aluminum surfaces. The presence of silver in the solder alloy of the paste permits the creation of a true intermetallic bond between the solder and the aluminum.

Applications: Superior Solder Paste AL26-SERIES is made from Type 3 Powder (-325/+500 Mesh Powder) with a unique flux binding system to keep the very active aluminum flux portion of the flux form degrading the solder powder. The material should be refrigerated before use and when in storage. The ideal temperature for printing and dispensing the paste is 20°C – 23°C with a relative humidity of 35-55%.

Information provided by Superior Flux

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.97 g/cc
Viscosity 280000 - 480000 cP
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 - 138 °CAlloy
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 195 °CSoldering Range
Shelf Life 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Superior Flux Superior Solder Paste ASP Direct Aluminum Solder Paste
Superior Flux Superior ASP-LT Direct Aluminum Solder Paste
Superior Flux Superior AL26-Series Direct Aluminum Solder Paste
Superior Flux Superior AL261-143-75 Direct Aluminum Solder Paste

NSFLUX102 / 185786

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.