MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Meldin Supplier

(Viewing data as-entered. Click here to return)
DuPont Mobility and Materials Vespel® ST-2030 DF Polyimide
Categories: Polymer; Thermoplastic; Polyimide, Thermoplastic; Thermoplastic Polyimide, Graphite Filled

Material Notes: Parts from nominal 30% (wt) graphite filled PI (polyimide) for high thermal oxidative stability combined with toughness and strength

Information provided by DuPont. This product line has remained with DuPont after the DuPont-Dow merger.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.44 g/ccASTM D 792
Filler Content 30 %
Water Absorption 0.50 %Immersion 24h; ASTM D 570
 1.3 %
@Temperature 50.0 °C
Immersion 48h; ASTM D 570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 57.0 MPa
@Temperature 23.0 °C
ASTM D 638
Elongation at Break 4.9 %
@Temperature 23.0 °C
ASTM D 638
Tensile Modulus 3927 MPa
@Temperature 23.0 °C
ASTM D 638
Compressive Strength 155 MPaASTM D 695
Izod Impact, Notched 0.411 J/cm
@Temperature 23.0 °C
ASTM D 256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 3.00e+6 ohm-cmASTM D 257
Surface Resistance 2.00e+7 ohmASTM D 257
Dielectric Constant 24.31
@Frequency 1e+6 Hz,
Temperature 23.0 °C
ASTM D 150
 36.25
@Frequency 10000 Hz,
Temperature 23.0 °C
ASTM D 150
 61.98
@Frequency 100 Hz,
Temperature 23.0 °C
ASTM D 150
Dissipation Factor 0.14236
@Frequency 1e+6 Hz
ASTM D 150
 0.1493
@Frequency 10000 Hz
ASTM D 150
 0.31044
@Frequency 100 Hz
ASTM D 150
 
Descriptive Properties
FillerGraphite Powder
Heat StabilizedYes
Polymer FamilyPolyimide
Polymer TypePI
Region AvailableAmericas
 Asia/Pacific
 Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M 4604 Silicone Rubber Termination Kit
DuPont Mobility and Materials VESPEL TP-8054 Polyimide
DuPont Mobility and Materials VESPEL TP-8169 Polyimide
DuPont Mobility and Materials VESPEL TP-8929 Polyimide
DuPont Mobility and Materials Vespel® SCP-5000 ISO Polyimide

PDTA7762 / 89876

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.