MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

3H Vinacom XLPE compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Description: 3H VINACOM HA-5010 is a silane cross-linkable polyethylene compound for low voltage electrical wire and cable insulation. Both the grafting and wire coating process are performed in one single step in the usual wire and cable production extruder for polyethylene and cross-linking takes place through a reaction involving water vapor after being extruded. Difficulty in maintaining dimensional accuracy during cross-linking is avoided because the temperature of crosslinking is below the crystalline melting point of the polymer. Therefore, 3H VINACOM XLPE HA-5010 allow cross-linked polyethylene wire and cable without the need for much capital in special equipment like peroxide or radiation cross-linking.

Applications: HA-5010 SA is suitable for below 10 kva or low voltage cables complying with the standard of IEC 60502 or TCVN 5935.

Information provided by 3H Vinacom

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³Value; ISO 1183
 0.920 - 0.940 g/cc0.0332 - 0.0340 lb/in³Standard; ISO 1183
Storage Temperature 10.0 - 30.0 °C50.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 0.123 MPa>= 17.8 psiStandard; IEC 60502; TCVN 5935
 0.191 MPa27.7 psiValue; IEC 60502; TCVN 5935
 >= 0.0981 MPa
@Temperature 136 °C,
Time 605000 sec
>= 14.2 psi
@Temperature 277 °F,
Time 168 hour
Standard, After aging; IEC 60502; TCVN 5935
 0.18167 MPa
@Temperature 136 °C,
Time 605000 sec
26.349 psi
@Temperature 277 °F,
Time 168 hour
Value, After aging; IEC 60502; TCVN 5935
Elongation at Break >= 200 %>= 200 %Standard; IEC 60502; TCVN 5935
 620 %620 %Value; IEC 60502; TCVN 5935
 >= 160 %
@Temperature 136 °C,
Time 605000 sec
>= 160 %
@Temperature 277 °F,
Time 168 hour
Standard, After aging; IEC 60502; TCVN 5935
 558 %
@Temperature 136 °C,
Time 605000 sec
558 %
@Temperature 277 °F,
Time 168 hour
Value, After aging; IEC 60502; TCVN 5935
Heat Distortion  5.0 %
@Pressure 0.200 MPa,
Temperature 200 °C
5.0 %
@Pressure 29.0 psi,
Temperature 392 °F
SET, Value; IEC 60502; TCVN 5935
 <= 15 %
@Pressure 0.200 MPa,
Temperature 200 °C
<= 15 %
@Pressure 29.0 psi,
Temperature 392 °F
SET, Standard; IEC 60502; TCVN 5935
 95 %
@Pressure 0.200 MPa,
Temperature 200 °C
95 %
@Pressure 29.0 psi,
Temperature 392 °F
HOT, Value; IEC 60502; TCVN 5935
 <= 175 %
@Pressure 0.200 MPa,
Temperature 200 °C
<= 175 %
@Pressure 29.0 psi,
Temperature 392 °F
HOT, Standard; IEC 60502; TCVN 5935
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+12 ohm-cm>= 1.00e+12 ohm-cmStandard; IEC 60502; TCVN 5935
 1.00e+15 ohm-cm1.00e+15 ohm-cmValue; IEC 60502; TCVN 5935
Dielectric Constant  2.3
@Frequency 1000 Hz
2.3
@Frequency 1000 Hz
Standard; ASTM D150
 2.3
@Frequency 1000 Hz
2.3
@Frequency 1000 Hz
Value; ASTM D150
Dissipation Factor  0.00025
@Frequency 60 Hz
0.00025
@Frequency 60 Hz
Standard; ASTM D150
 0.00025
@Frequency 60 Hz
0.00025
@Frequency 60 Hz
Value; ASTM D150
 
Thermal PropertiesMetricEnglishComments
Shrinkage 0.00 - 0.025 %0.00 - 0.025 %IEC 60502; TCVN 7447:1998
 <= 0.040 %<= 0.040 %IEC 60502; TCVN 7447:1998
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 °C320 °FC1
 170 °C338 °FC2
 185 °C365 °FC3
 195 °C383 °FC4
 200 °C392 °FC5
 205 °C401 °FNeck
Die Temperature 285 °C545 °F
Head Temperature 210 °C410 °F
Shelf Life 6.00 Month6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PVINAC000 / 249349

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.