HIFOR Xtreme® SC74884 is an enhanced hexene LLDPE designed for blown film extrusion applications requiring high strength and toughness. HIFOR Xtreme® SC74884 contains no slip or anti-block. This material is highly stabilized and contains process aid. This product has some 21 CFR clearances. Application/Uses: Blown film extrusion, Heavy Duty Films.Information provided by Westlake Chemical Corporation. |