MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vinnolit® C 12/62 V Vinyl Chloride/Vinyl Acetate Copolymer Extender resin
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: Vinnolit® C 12/62 V Vinyl chloride/vinyl acetate copolymer extender resin for paste application. Vinnolit® C 12/62 V is a copolymeric extender resin having a high vinyl acetate content which has been specially developed for paste making. In blends with paste-making PVC resins, it combines the good viscosity-reducing properties of the homopolymer paste extender resins with the lower gelling temperatures typical of vinyl acetate copolymers. By incorporating an extender resin such as Vinnolit® C 12/62 V processing can be improved as the viscosity is considerably reduced, particularly in low plasticizer content and highly filled plastisols. By exchanging part of a copolymer paste resin the shelf life and deaeratibility are improved and dilatancy is reduced. The higher vinyl acetate content of Vinnolit® C 12/62 V allows lower gelling temperatures. The adhesion to various substrates, such as metal and synthetic fibers is improved. Vinnolit® C 12/62 V is particularly well suited for automotive underbody coatings and sealants, carpet backing and laminating pastes. Like all extender resins Vinnolit® C 12/62 V can be processed by all the standard methods, such as coating, dipping, casting and spraying.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.50 %ISO 1269
Apparent Bulk Density 0.650 g/ccISO 60
Particle Size <= 100 µm<= 0.5% Retained on 0.1 mm Sieve; DIN EN ISO 53195
Viscosity Test 0.95 dl/gReduced Viscosity; ISO 1628-2
Vinyl Acetate Content 12 %
 
Descriptive Properties
K-Value62ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVINNO920 / 291117

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.