MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BYK Fluacolor® DC Clay
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes:
  • Fulacolor DC is a high performance reactive acid clay, produced using advanced acid activation and surface modification technology delivering excellent dispersion properties to high solids.
  • Fulacolor DC is compatible with all capsule technologies to produce a high definition instantaneous image. Low coarse particle content minimizes abrasion and capsule bleed, and extends filter-cycles.
  • Fulacolor DC is a non-toxic material produced from natural material and consequently has extremely low environmental impact.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 26.5 lb/ft³aerated
 36.8 lb/ft³tapped
Particle Size 4.2 - 5.0 µmMean
pH 6.0 - 8.02% suspension in water
Viscosity <= 200 cP40% solids @ pH
 
Component Elements PropertiesOriginal ValueComments
H2O, Water 5.0 - 11 %
 
Descriptive Properties
Whiteness>86%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Cloisite® 30B Bentonite
BYK Cloisite® 30B Nanoclay
BYK Cloisite® 5 Salt with bentonite
BYK Cloisite® 93 Salt with bentonite
BYK Cloisite® 93A Nanoclay

PBYK042 / 185039

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.