MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

BASF 3D Ultrafuse® ABS Fusion+ Fused Fillament
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ABS Polymer

Material Notes: Components: Acrylonitrile Butadiene Styrene based filament for Fused Filament Fabrication.

Product Description: ABS Fusion? made with Polyscope XILOY™ 3D is an engineering filament which has been optimized for 3D-printing. This special grade has been developed in collaboration with Polyscope Polymers - renowned for its material solutions in the automotive industry. ABS is a thermoplastic which is used in many applications. Although ABS has been classified as a standard material in 3D-printing it is known to be quite challenging to process. ABS Fusion+ combines the properties of ABS with an improved processability. The filament is based on an ABS grade which can be directly printed on glass without any adhesives or tape and has a higher success rate of prints due to extreme low warping.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.075 g/cc0.03884 lb/in³Printed Part; ISO 1183-1
Melt Flow 10.75 g/10 min
@Load 5.00 kg,
Temperature 250 °C
10.75 g/10 min
@Load 11.0 lb,
Temperature 482 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 17.9 MPa2600 psiZX: Upright; ISO 527
 29.5 MPa4280 psiXY: Flat; ISO 527
Elongation at Break 2.1 %2.1 %ZX: Upright; ISO 527
 10.9 %10.9 %XY: Flat; ISO 527
Modulus of Elasticity 1.106 GPa160.4 ksiYoung's, ZX: Upright; ISO 527
 1.379 GPa200.0 ksiYoung's, XY: Flat; ISO 527
Flexural Strength 23.1 MPa3350 psiZX: Upright; ISO 178
 48.3 MPa7010 psiXY: Flat; ISO 178
 48.7 MPa7060 psiXZ: On its edge; ISO 178
Flexural Modulus 0.878 GPa127 ksiZX: Upright; ISO 178
 1.133 GPa164.3 ksiXZ: On its edge; ISO 178
 1.406 GPa203.9 ksiXY: Flat; ISO 178
Flexural Strain at Break 2.7 %2.7 %ZX: Upright; ISO 178
 5.6 %5.6 %XY: Flat; ISO 178
 5.9 %5.9 %XZ: On its edge; ISO 178
Izod Impact, Notched (ISO) 2.20 kJ/m²1.05 ft-lb/in²ZX: Upright; ISO 180
 26.4 kJ/m²12.6 ft-lb/in²XY: Flat; ISO 180
 38.4 kJ/m²18.3 ft-lb/in²XZ: On its edge; ISO 180
Izod Impact, Unnotched (ISO) 6.60 kJ/m²3.14 ft-lb/in²ZX: Upright; ISO 180
 73.1 kJ/m²34.8 ft-lb/in²XY: Flat; ISO 180
 131.1 kJ/m²62.38 ft-lb/in²XZ: On its edge; ISO 180
Charpy Impact Unnotched 0.690 J/cm²3.28 ft-lb/in²ZX: Upright; ISO 179-2
 7.19 J/cm²34.2 ft-lb/in²XY: Flat; ISO 179-2
 11.87 J/cm²56.48 ft-lb/in²XZ: On its edge; ISO 179-2
Charpy Impact, Notched 0.250 J/cm²1.19 ft-lb/in²ZX: Upright; ISO 179-2
 3.20 J/cm²15.2 ft-lb/in²XY: Flat; ISO 179-2
 4.19 J/cm²19.9 ft-lb/in²XZ: On its edge; ISO 179-2
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C196 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 71.0 °C160 °FISO 75-2
Glass Transition Temp, Tg 114 °C237 °FISO 11357-2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 100 - 120 °C212 - 248 °FBed, Bed Material: Glass
Nozzle Temperature 240 - 260 °C464 - 500 °F
Drying Temperature 60.0 °C140 °Fin a hot air dryer or vacuum oven
Dry Time 4.00 - 16.0 hour4.00 - 16.0 hour
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Nozzle Diameter=0.4 mm
Print speed40-80 mm/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PBASF3D007 / 312248

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.