MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Envalior Durethan® DP 1100/30 H2.0 901510 Nylon 6 (PA6), 30% Micro bead Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass Bead Filled

Material Notes: 30% micro beads, improved surface finish

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.351 g/cc0.04881 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.0107 cm/cm0.0107 in/in150x105x3; ISO 2577
Linear Mold Shrinkage, Transverse 0.0113 cm/cm0.0113 in/in150x105x3; ISO 2577
Melt Flow 28 g/10 min
@Load 5.00 kg,
Temperature 280 °C
28 g/10 min
@Load 11.0 lb,
Temperature 536 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 175 MPa25400 psiISO 2093-1
Tensile Strength at Break 75.0 MPa10900 psi5 mm/min; ISO 527-1,-2
Tensile Strength, Yield 80.0 MPa11600 psi50 mm/min; ISO 527-1,-2
Elongation at Break 5.0 %5.0 %5 mm/min; ISO 527-1,-2
Elongation at Yield 3.5 %3.5 %50 mm/min; ISO 527-1,-2
Tensile Modulus 4.30 GPa624 ksi1 mm/min; ISO 527-1,-2
Flexural Strength 125 MPa18100 psi2 mm/min; ISO 178-A
Flexural Yield Strength 115 MPa
@Strain 3.5 %
16700 psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 3.90 GPa566 ksi2 mm/min; ISO 178-A
Flexural Strain at Break 5.0 %5.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) 3.50 kJ/m²
@Temperature 23.0 °C
1.67 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)  20.0 kJ/m²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
 20.0 kJ/m²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
Charpy Impact Unnotched  2.00 J/cm²
@Temperature -30.0 °C
9.52 ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact, Notched 0.300 J/cm²
@Temperature 23.0 °C
1.43 ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 75.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow 75.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
41.7 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Deflection Temperature at 0.46 MPa (66 psi) 180 °C356 °FISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FISO 75-1,-2
Deflection Temperature at 8.0 MPa 50.0 °C122 °FISO 75-1,-2
Vicat Softening Point 205 °C
@Load 5.10 kg
401 °F
@Load 11.2 lb
120°C/h; ISO 306
Shrinkage, MD 0.31 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.31 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 2577
Shrinkage, TD 0.31 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.31 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 2577
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °F
Mold Temperature 80.0 °C176 °F
Back Pressure 50.0 MPa7250 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLANW9550 / 208309

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.