MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Maxxam™ 8400-7001 Polypropylene with 30% Calcium Carbonate  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Calcium Carbonate (CaCO3) Filler

Material Notes: Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Filler Content 30 %
Linear Mold Shrinkage, Flow 0.010 - 0.018 cm/cmASTM D955
Melt Flow 280 g/10 min
@Load 2.16 kg,
Temperature 200 °C
Procedure A; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 17.9 MPaType I, 51 mm/min; ASTM D638
Elongation at Break 100 %Type I, 51 mm/min; ASTM D638
Flexural Strength 28.3 MPaASTM D790
Flexural Modulus 1520 MPaASTM D790
Izod Impact, Notched 107 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
@Thickness 3.18 mm
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 54.4 °C
@Thickness 3.18 mm
Annealed; ASTM D648
 
Descriptive Properties
AppearanceGray
FeaturesCopolymer
 General Purpose
FormsPellets
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesConstruction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Matrixx CPP1B30 Polypropylene Homopolymer, 30% Calcium Carbonate Filled
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder
A. Schulman Fiberfil® PP-60/CC/30 Polypropylene Homopolymer, 30% Calcium Carbonate
Buckeye Polymers BP RPP 2011 C Polypropylene, 20% Mineral Filled
Alcoa KAMA 7120 Calcium Carbonate Filled Homopolymer Polypropylene (PP)

PH1PN9106 / 102942

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.