MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PS CPDS FT876 Flame Retardant Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: POLYSTYRENE (PS) COMPOUND (CPDS) FT876 is a high impact, halogen free flame retardant polystyrene with good thermal stability and processability.

Main Characteristics:

  • Bromine and Chlorine free,
  • UL94 V0 @ 2.5 mm,
  • High heat and good thermal and UV stability.

Applications: Television covers, Decoders, Hi-Fi, Office automation.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.10 g/ccISO 1183
Water Absorption <= 0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
Melt Flow 3.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ISO 1133H
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPaISO 527-2
Tensile Strength, Yield 30.0 MPaISO 527-2
Elongation at Break 40 %ISO 527-2
Flexural Modulus 2300 MPaISO 178
Izod Impact, Notched (ISO) 6.00 kJ/m²180/1A
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 85.0 °C
@Load 5.10 kg
50°C per hour; ISO 306B50
Flammability, UL94 V-0
@Thickness 2.50 mm
Black and Gray
 
Processing PropertiesOriginal ValueComments
Melt Temperature <= 280 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa FRHIPS-702 Flame Retardant Polystyrene
Total PS CPDS 856 Flame Retardant Polystyrene
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded

PTOTAL903 / 130628

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.