Description: Braskem Flexus7200 is a Linear Low Density Polyethylene, metallocene ethylene-hexene copolymer, produced by gas fase process. It was specially designed to provide outstanding processing performance. Films obtained with this grade show excellent impact and puncture resistances. It contains antioxidant additives. Applications: Stretch films; Liners; LDPE and HDPE blends; Packages for general use. Information provided by Braskem. |