MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Niche Polymer POLIXL™ PA66GI14BK PA66, 14% Fiberglass Reinforced, Impact Modified
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 10% Glass Fiber Filled; Nylon 66, Impact Grade

Material Notes:

Information provided by Niche Polymer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D792
Moisture Absorption at Equilibrium 1.8 %1.8 %50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm0.0090 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inASTM D955
Ash 14 %14 %glass-fiber; ASTM D2584
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 110 MPa16000 psiISO 527
Elongation at Break 5.0 %5.0 %ISO 527
Flexural Strength 165 MPa23900 psiISO 178
Flexural Modulus 5.51 GPa799 ksiISO 178
Izod Impact, Notched (ISO)  11.0 kJ/m²
@Temperature -30.0 °C
5.23 ft-lb/in²
@Temperature -22.0 °F
ISO 180
 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FUnannealed; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 240 °C464 °FUnannealed; ISO 75
Flammability, UL94  HB
@Thickness 0.750 mm
HB
@Thickness 0.0295 in
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Plastcom SLOVAMID 66 GF 14 HI TS PA66, 14% glass fibre, improved strength
DuPont Mobility and Materials Zytel® 8018HS NC010 PA66-IGF14
Celanese Zytel® 8018HS BKB085 PA66-IGF14
Polykemi AB SCANAMID 66 A43^E F14 Nylon 66, Glass Fiber Reinforced, Modified
Akro-Plastic Akromid® A3 GF 30 S1 black (3723) PA66-I Conditioned

PNICHE144 / 193726

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.