A specially developed Polyvinyl Alcohol (PVA) 3D printer filament that is ideally used as a water soluble support material. General properties: - Water soluble
- Good flowing thermoplastic
- Safe to print
Applications:- As a support material for other 3D printer filaments
Information provided by Clariant. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.Click here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |