MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Covestro Desmopan® 85085A DPS 055 TPU
Categories: Polymer; Thermoplastic; Polyurethane, TP

Material Notes: Injection molding grade; no yellowing under the action of UV light; improved microbial resistance; good low-temperature flexibility; Improved hydrolysis resistance; Application; automotive interior applications

Mechanical property data for samples at 50% RH.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/ccISO 1183-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 85ISO 868
Tensile Strength, Ultimate 4540 psi200 mm/min; DIN 53504
Elongation at Break 623 %200 mm/min; DIN 53504
Tensile Modulus 55.0 MPa
@Temperature 60.0 °C
storage; ISO 6721-1,-4
 86.0 MPa
@Temperature 20.0 °C
storage; ISO 6721-1,-4
 207 MPa
@Temperature -20.0 °C
storage; ISO 6721-1,-4
50% Modulus 0.00510 GPa
@Strain 50 %
200 mm/min; DIN 53504
100% Modulus 0.00640 GPa
@Strain 100 %
200 mm/min; DIN 53504
200% Modulus 0.0107 GPa
@Strain 200 %
200 mm/min; DIN 53504
Rebound 63 %Resilience; ISO 4662
Tear Strength 75.0 kN/m500 mm/min; ISO 34-1
Abrasion 28mm3; ISO 4649 method A
Compression Set 18 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 23 %
@Temperature 70.0 °C,
Time 86400 sec
DIN ISO 815-1, Method C
 40 %
@Temperature 70.0 °C,
Time 86400 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Melt Temperature 180 - 210 °C
Mold Temperature 20.0 - 40.0 °C
Drying Temperature 80.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 3378A TPU
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
Covestro Desmopan® 9370A Thermoplastic Polyurethane
Covestro Texin® 285 Thermoplastic Polyurethanes (TPU)
PlastiComp Complet® LCF40 - ETPU Rigid Thermoplastic Polyurethane, 40% Long Carbon Fiber Reinforced

PCOVEST0731 / 202514

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.