MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

H.C. Starck NRC® 4N5 (UNS R05200) Electron Beam Melted Tantalum
Categories: Metal; Nonferrous Metal; Refractory Metal; Pure Element

Material Notes: Applications: NRC® ETA Tantalum metal products are used where purity and or ductility of the tantalum metal is more important than strength or grain size. Consequently, their primary applications are in sputtering, nickel based superalloys, explosion bonding of liners for corrosion resistance, medical, and ordnance applications All grades meet ASTM requirements.

Forms Available: Sheet, Plate, Tube, Rod, Wire and Bar.

Typical Purity: Purity refers to 100% minus total metallic content only, gases are omitted from the calculation. Metallic impurities are measured by GDMS, gases by Leco.

Metallurgical Characteristics: Material is single-phase tantalum. Stress relieve at 1500°F, re-crystallize at 1900°F - 2100°F.

Information provided by H.C. Starck.

Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 16.6 g/cc0.600 lb/in³
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 180.95180.95
Atomic Number 7373
Thermal Neutron Cross Section 21.3 barns/atom21.3 barns/atom
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B 25 - 6525 - 65hardness as annealed, typical
Hardness, Vickers 80 - 12080 - 120hardness as annealed, typical
Tensile Strength, Ultimate 241 - 310 MPa35000 - 45000 psitypical
Tensile Strength, Yield 138 - 207 MPa20000 - 30000 psitypical
Modulus of Elasticity 186 GPa27000 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 0.0000147 ohm-cm
@Temperature 0.000 - 100 °C
0.0000147 ohm-cm
@Temperature 32.0 - 212 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 6.48 µm/m-°C
@Temperature 20.0 - 500 °C
3.60 µin/in-°F
@Temperature 68.0 - 932 °F
Specific Heat Capacity 0.141 J/g-°C
@Temperature 100 °C
0.0336 BTU/lb-°F
@Temperature 212 °F
Thermal Conductivity 55.3 W/m-K
@Temperature 20.0 - 100 °C
384 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
Melting Point 2996 °C5425 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al <= 0.00010 %<= 0.00010 %
Cadmium, Cd <= 0.00010 %<= 0.00010 %
Calcium, Ca <= 0.00010 %<= 0.00010 %
Carbon, C <= 0.0040 %<= 0.0040 %
Chlorine, Cl <= 0.00010 %<= 0.00010 %
Chromium, Cr <= 0.00010 %<= 0.00010 %
Cobalt, Co <= 0.00010 %<= 0.00010 %
Copper, Cu <= 0.00010 %<= 0.00010 %
Hafnium, Hf <= 0.00010 %<= 0.00010 %
Hydrogen, H <= 0.0010 %<= 0.0010 %
Iron, Fe <= 0.00010 %<= 0.00010 %
Lead, Pb <= 0.00010 %<= 0.00010 %
Lithium, Li <= 0.00010 %<= 0.00010 %
Magnesium, Mg <= 0.00010 %<= 0.00010 %
Manganese, Mn <= 0.00010 %<= 0.00010 %
Molybdenum, Mo <= 0.0015 %<= 0.0015 %
Nickel, Ni <= 0.00010 %<= 0.00010 %
Niobium, Nb (Columbium, Cb) <= 0.0040 %<= 0.0040 %
Nitrogen, N <= 0.0040 %<= 0.0040 %
Other, each <= 0.00010 %<= 0.00010 %
Oxygen, O <= 0.010 %<= 0.010 %
Potassium, K <= 0.00010 %<= 0.00010 %
Silicon, Si <= 0.00010 %<= 0.00010 %
Sodium, Na <= 0.00010 %<= 0.00010 %
Sulfur, S <= 0.00010 %<= 0.00010 %
Tantalum, Ta >= 99.995 %>= 99.995 %Balance
Thorium, Th <= 5.0e-7 %<= 5.0e-7 %
Tin, Sn <= 0.00010 %<= 0.00010 %
Titanium, Ti <= 0.00010 %<= 0.00010 %
Tungsten, W <= 0.0030 %<= 0.0030 %
Uranium, U <= 5.0e-7 %<= 5.0e-7 %
Vanadium, V <= 0.00010 %<= 0.00010 %
Yttrium, Y <= 0.00010 %<= 0.00010 %
Zinc, Zn <= 0.00010 %<= 0.00010 %
Zirconium, Zr <= 0.00010 %<= 0.00010 %
 
Descriptive Properties
Total Metallic Content<0.005%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Tantalum, UNS R05200
Sharadaa Ceramics 29 Insulation Bricks-ASTM
Sharadaa Ceramics 26 Insulation Bricks-ASTM
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded

NHCST933 / 130823

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.