MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici Torzen ® Marathon G3500XHL BK34 Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: PA66 35% glass fiber reinforced, injection molding grade with enhanced thermal resistance in contact with hot air. High improvement of mechanical properties retention versus standard polyamide 66 after heat aging. Black color.

Suitable for parts requiring high stiffness, good mechanical resistance and good heat aging properties retention.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³DAM; ISO 1183
Water Absorption  1.1 %
@Thickness 2.00 mm,
Time 86400 sec
1.1 %
@Thickness 0.0787 in,
Time 24.0 hour
Immersion @ 23°C; ISO 62
 2.0 %
@Thickness 1.00 mm,
Time 86400 sec
2.0 %
@Thickness 0.0394 in,
Time 24.0 hour
Immersion; ISO 62
Moisture Absorption 1.70 %
@Thickness 2.00 mm,
Temperature 23.0 °C
1.70 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 210 MPa30500 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.0 %3.0 %5 mm / min. DAM; ISO 527-2/1A
Tensile Modulus 11.5 GPa1670 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 320 MPa46400 psi2mm / min. DAM; ISO 178
Flexural Modulus 10.5 GPa1520 ksi2mm / min. DAM; ISO 178
Izod Impact, Unnotched (ISO) 12.0 kJ/m²5.71 ft-lb/in²ISO 180/1U
Charpy Impact, Notched 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 
Thermal PropertiesMetricEnglishComments
Melting Point 262 °C504 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75/2Af
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 300 °C536 - 572 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
Injection Molding Injection SpeedMedium - high

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6973 / 293478

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.