MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
GEHR Plastics PVC-HI Polyvinylchloride, Impact Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, High Impact

Material Notes: Polyvinyl chloride is a flame retardant material with an exceptional chemical resistance and also with lower stress cracking. PVC-U shows high mechanical strength, tensile strength and the continuous operating temperature is from -15°C to 60°C. It can also be easily solvent, cemented and welded.

Properties include:

  • High mechanical strength, tensile strength and hardness
  • Good insulation properties for electronics
  • High chemical resistance
  • Self-extinguishing
  • Low water absorption
  • Easy to varnish and glue
  • Low impact strength
  • Limited weather resistance
Applications include:
  • Pumps and valve body
  • Gaskets
  • Bearing cages
  • Pipe lines
  • Hand pump pipes
  • Brush basic body
  • Parts in the dental medicine
  • Seat strips
  • Pipes for the mounting of kerfs
  • Lamp box
PVC-HI has increased impact strength at low temperatures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.38 g/ccISO 1183
Water Absorption at Saturation 0.20 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 78DIN 53505
Ball Indentation Hardness 100 MPaISO 2039-1
Tensile Strength at Break 30.0 MPaISO 527
Tensile Strength, Yield 49.0 MPaISO 527
Elongation at Break 30 %ISO 527
Elongation at Yield 10 %ISO 527
Modulus of Elasticity 2.60 GPaISO 527
Flexural Strength 80.0 MPaISO 178
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 10.0 kJ/m²ISO 179
Coefficient of Friction 0.60DIN 53375
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmVDE 0303
Surface Resistance 1.00e+13 ohm
Dielectric Constant 3.0
@Frequency 1e+6 Hz
Dielectric Strength 20.0 - 40.0 kV/mmVDE 0303
Dielectric Loss Index 0.010
@Frequency 1e+6 Hz
DIN 53483
Comparative Tracking Index 600 VKB; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°CDIN 53752
Thermal Conductivity 0.170 W/m-K
@Temperature 20.0 °C
Maximum Service Temperature, Air 60.0 °C
Deflection Temperature at 0.46 MPa (66 psi) 69.0 °CISO 75
Vicat Softening Point 78.0 °CVST/B/50; ISO 306
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-0UL 94
 
Descriptive Properties
Acid Resistanceyes
Aromatic Resistancelimited
Bondabilityyes
Chemical ResistanceDIN 8061
CKW Resistanceno
Hydrocarbonate Resistanceyes
Hydroxide Resistanceyes
Ketone Resistanceno
Resistance Against Hot Waterno
UV Stabilizationfair

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Novatec Novablend® 6701 PVC
Geon® Performance Solutions Vinyl Dry Blend E7857 PVC, Rigid
Geon® Performance Solutions Vinyl Dry Blend E1893 PVC, Rigid
GEHR Plastics PVC-U Polyvinylchloride
Hippe PA 46 Nylon 46

PGEHR002 / 79839

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.