MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Precision Polymer Engineering R60R Natural Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Natural Rubber & Kevlar® NR6F722, 55-65 °IRHD. ASTM D1418 designation: NR. Kevlar® is a registered trademark of DuPont. ASTM D2000/SAE J200 Type, Class: AA.

Applications: Natural rubber offers low compression set, high tensile strength, high resilience and excellent resistance to tear and abrasion. Natural rubber also offers excellent adhesion to metals. Good resistance to a range of organic acids and alcohol’s, with moderate resistance to aldehydes. Poor against weathering, ozone and petroleum based oils.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60°IRHD; ASTM D1415
Tensile Strength, Yield 19.0 MPaASTM D412
Elongation at Break 515 %ASTM D412
Compression Set 40 %
@Temperature 70.0 °C,
Time 86400 sec
ASTM D395
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °C
Minimum Service Temperature, Air -50.0 °C
 -40.0 °CNon-brittle after 3 minutes
Flash Point >= 300 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Precision Polymer Engineering E50Q Ethylene Propylene Rubber
Precision Polymer Engineering N75L Nitrile Rubber
Precision Polymer Engineering N70L Nitrile Rubber
Precision Polymer Engineering N70M Nitrile Rubber
Precision Polymer Engineering E60Q Ethylene Propylene Rubber

PPRECI169 / 57893

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.