MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil ACHIEVE 3854 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Product Description: A premium homopolymer resin produced using ExxonMobil Chemical’s Exxpol™ Technology designed specifically for spunbpond technology. Narrow molecular weight distribution of the resin allows for excellent uniformity, finer fibers and high tensile strength allowing for creative innovations in applications and possible downgauging.

Availability: North America and South America

Features:

  • Clean/High Purity
  • Low Smoke Emission
Uses:
  • Personal Care
  • Spunbond Nonwovens
  • Textile Applications
Processing Method: Fiber (Spinning) Extrusion and Filament Extrusion

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/cc
Melt Flow 24 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil ACHIEVE 3825 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications
ExxonMobil PP1024E4 Homopolymer
ExxonMobil PP3155 Homopolymer Grade for Nonwoven and Fiber Applications
BP Amoco Accpro® 9117 Enhanced Polypropylene
Braskem HP 525M Film Extrusion Polypropylene

PEXB296 / 37601

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.