Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America Filler/Reinforcement: Glass Fiber, 40% Filler by Weight Additive: Heat Stabilizer Features: Heat Stabilized; High Impact Resistance Uses: Appliance Components; Automotive Applications; Automotive Interior Parts; Electrical/Electronic Applications RoSH Compliance: RoSH Compliant Forms: Granules Processing Method: Injection Molding Information provided by EMS-Grivory |