MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Phillips Sumika Marlex® CBF-265 Thermoplastic Polyolefin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Mineral Reinforced

Material Notes: Talc-Filled, High Flow, Thermoplastic Polyolefin.

Applications: Automotive Exterior Parts

Conditioning after Molding: 48 hr at 23°C

Nominal Shrinkage: 0.8-1.0%

    Drying conditions
  • Temperature: 80-100°C
  • Time: 2 hours minimum, 4 hours maximum
  • Device: Desiccant Dryer
  • Moisture content: 0.1 wt% max.

    Molding Temperatures
  • Rear Temperature: 145-200°C
  • Middle Temperature: 210-235°C
  • Front and Nozzle Temps: 210-235°C
  • Stock Temperature: 191-246°C
  • Mold Temperature: 23-50°C

    Processing conditions
  • Suggested shot size: 50-70%
  • First stage injection pressure: Maximize
  • Screw Speed: 30-60%
  • Packing pressure: Minimize
  • Back Pressure: 50-150 psi

Other molding considerations: Melt temperature above 260°C may cause resin degradation and changes to resin properties. To improve dispersion of color concentrates use a screw with a mixing zone or mixing nozzle.

Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.

Key Words: Information Provided by Chevron Phillips Chemical
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.960 g/cc0.0347 lb/in³ISO 1183
Linear Mold Shrinkage 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/in
Melt Flow 26 g/10 min
@Temperature 230 °C
26 g/10 min
@Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ISO 868
Tensile Strength, Yield 16.0 MPa2320 psi50 mm/min; ISO 527
Flexural Modulus 1.05 GPa152 ksi2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 44.0 kJ/m²20.9 ft-lb/in²ISO 180
 4.00 kJ/m²
@Temperature -40.0 °C
1.90 ft-lb/in²
@Temperature -40.0 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C117 °FISO 75

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPPP003 / 90440

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.