DURAFLEX TPV63HC is 63 shore A durometer Thermoplastic Vulcanizate (TPV) that is ISO10993 compliant. This grade is designed for use in medical applications. This grade is available in natural and black. Available in AMR, EUR, and PAC.Information provided by Conventus Polymers LLC |