MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ethyl acrylate, C5H8O2
Categories: Fluid; Solvent

Key Words: C5H8O2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/cc
@Temperature 20.0 °C
Viscosity 0.615 cP
@Temperature 20.0 °C
Dynamic Viscosity
Molecular Weight 100.118 g/mol
Vapor Pressure 30.867 torr
@Temperature 20.0 °C
 
Chemical PropertiesOriginal ValueComments
Critical Pressure 37.0 atm
Critical Temperature 279 °C
Critical Density 0.313 g/cc
Critical Molar Volume 320 cm³/mol
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 447.2 J/g
Thermal Conductivity 0.1458 W/m-K
@Temperature 20.0 °C
Melting Point -72.2 °C
Boiling Point 99.9 °C
 
Descriptive Properties
Antoine's Vapor Pressure A Parameter16.089
Antoine's Vapor Pressure B Parameter2974.94
Antoine's Vapor Pressure C Parameter-58.15
Antoine's Vapor Pressure Formulaln πp = A - B/(T+C)P in mmHg and T in K
CAS registry number (CARN)140-88-5
Chemical FormulaC5H8O2
Critical Compressibility (Zc)0.261
Dipole moment (p/C.m)none
Dynamic Viscosity Formulalog10 η=A(1/T-1/B)
Dynamic Viscosity Parameter A438.04
Dynamic Viscosity Parameter B256.84
Molar Heat Capacity of Vapor a Parameter16.7988
Molar Heat Capacity of Vapor b Parameter3.6874
Molar Heat Capacity of Vapor c Parameter-0.0001381
Molar Heat Capacity of Vapor d Parameter-5.728E-09
Molar Heat Capacity of Vapor FormulaCp = a + bT + cT2 + dT3Cp in J/mol-K
UN Number1917

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

VORGS162 / 99537

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.