A 30% glass fiber, thermostabilized polybutylene terephthalate. Designed for injection molding and extrusion of various items and parts for construction, electrical tools, machine engineering, radio engineering and handles in gas device systems. Available in natural and black colors.Information provided by Polyplastic Compounds |