MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4300 G6 FC 30% Glass Filled PBT
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Description: The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including FDA, European Food Contact n°2002/72/EC and GMP (EC) n°2023/2006.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 - 0.900 g/cc
Density 1.53 g/ccISO 1183
Water Absorption 0.40 %ISO 62
Moisture Absorption at Equilibrium 0.20 %ISO 62
Viscosity Test 102 cm³/gISO 307
Linear Mold Shrinkage, Flow 0.0020 cm/cmplate with film gate 150x150x3mm3
 0.0034 cm/cmISO 2577
Linear Mold Shrinkage, Transverse 0.0107 cm/cmISO 2577
 0.011 cm/cm
Melt Flow 16.83 g/10 min
@Load 2.16 kg,
Temperature 250 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 190 MPa
@Load 98.0 kg,
Time 30.0 sec
ISO 2039-1
Tensile Strength at Break 140 MPaISO 527-1/-2
Elongation at Break 3.0 %ISO 527-1/-2
Tensile Modulus 9800 MPaISO 527-1/-2
Flexural Strength 200 MPaISO 178
Charpy Impact Unnotched 70.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
 74.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
Charpy Impact, Notched 9.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Tensile Creep Modulus, 1000 hours 7500 MPa
@Strain <=0.5 %
ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Constant 3.8
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
IEC 60250
Dissipation Factor 0.0025
@Frequency 100 Hz
IEC 60250
 0.017
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 VTest Solution B; IEC 60112
 375 VTest Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 20.0 - 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-1/-2
Thermal Conductivity 0.270 W/m-KDIN 52612-1
Melting Point 223 °CISO 11357-1/-2
Maximum Service Temperature, Air 140 °Cat 50% loss of tensile strength after 20,000hr
 160 °Cat 50% loss of tensile strength after 5,000hr
 210 °C
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 215 °CISO 75-1/-2
Decomposition Temperature >= 290 °C
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Diameter 4.00 mm
 HB
@Diameter 0.400 mm
Ignition Temperature 350 °CASTM D1929
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 275 °CInjection molding/Extrusion
Mold Temperature 60.0 - 100 °CInjection molding
 
Descriptive Properties
Commercial StatusEurope

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultradur® B 4300 G6 LT 30% Glass Filled BK 150926 PBT
BASF Ultradur® B 4300 G6 HR 30% Glass Filled BK 15116 PBT
BASF Ultradur® B 4500 BK 00110 PBT
BASF Ultradur® B 4300 G6 HR 30% Glass Filled PBT
BASF Ultradur® B 4330 G6 HR 30% Glass Filled PBT

PBASG0126 / 131759

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.