MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Bayshore Vinyl Compounds BRC R7560 CLR 221 PVC Compound, Food Grade
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: BRC R7560 CLR 221 is a food grade PVC bottle compound made with 100% FDA approved ingredients. This product exhibits excellent clarity and can be used in many applications where food contact is required. R 7560 CLR 221 contains no heavy metals, is California Prop 65 compliant, and complies with the European Lead Free directive, as well as RoHS (Restriction of Hazardous Substances).

Information Provided by Bayshore Vinyl Compounds Inc., a Mexichem Company.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.34 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 82ASTM D2240
Tensile Strength at Break 6680 psiASTM D638
Tensile Modulus 343 ksiASTM D638
Flexural Yield Strength 12.58 ksiASTM D790
Flexural Modulus 385 ksiASTM D790
Izod Impact, Unnotched 22.0 ft-lb/inASTM D256
Impact 4.7Gardner [in-lb/mil]; ASTM D5420
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 66.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Karina E 85/253-IS-SI-AT Compound PVC Crystal
Bayshore Vinyl Compounds BVC 1100-78 Clear PVC Compound
Bayshore Vinyl Compounds BRC R7550 CLR 223V Extrusion Compound
Karina 805-10/152-A-ERYB White PVC Compound
Karina 822-18/599-CRB-LMP Gray PVC Compound

PBAYS012 / 93284

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.