Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel. Availability: Africa & Middle East and Europe Additive: - Antiblock: No
- Slip: No
- Thermal Stabilizer: Yes
Applications:- Bag in Box
- Batch Inclusion Bags
- Blown Film
- Food packaging
- Protective Film
Information provided by ExxonMobil |