MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
RESPOL REPSOL PRIMEVA® P1820F EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Product Description: EVA copolymer REPSOL PRIMEVA® P1820F is suitable for film extrusion and extrusion coating. This material combines easy processability with excellent mechanical and optical properties. It contains antioxidant additives.
Applications: Film extrusion, Extrusion coating
Recommended melt temperature below 200°C to avoid the decomposition of the polymer. Processing conditions should be optimized for each production line.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Additive: Antioxidant

Features: Antioxidant; Copolymer; Food Contact Acceptable; Good Optical Properties; Good Processability

Uses: Coating Applications; Film

Agency Ratings: EU Food Contact

Processing Method: Extrusion Coating; Film Extrusion

Information provided by REPSOL

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.937 g/ccISO 1183
Environmental Stress Crack Resistance >= 300 hourF50; ASTM D1693
Vinyl Acetate Content 18 %
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 90ISO 868
Hardness, Shore D 38ISO 868
Film Elongation at Break, MD 320 %
@Thickness 0.0508 mm
ISO 527-3
Film Elongation at Break, TD 640 %
@Thickness 0.0508 mm
ISO 527-3
Elmendorf Tear Strength MD 204 g
@Thickness 0.0508 mm
ISO 6383-2
Elmendorf Tear Strength TD 281 g
@Thickness 0.0508 mm
ISO 6383-2
Dart Drop Test 600 gF50; ISO 7765-1
Film Tensile Strength at Break, MD 3770 psi
@Thickness 0.0508 mm
ISO 527-3
Film Tensile Strength at Break, TD 3190 psi
@Thickness 0.0508 mm
ISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 189 °F
Vicat Softening Point 147 °FISO 306/A
 
Optical PropertiesOriginal ValueComments
Haze 4.0 %ASTM D1003
 
Processing PropertiesOriginal ValueComments
Melt Temperature 392 °F
Blow-up Ratio (BUR) 2.25

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRESPOL1322 / 312015

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.