Carbon fiber reinforced for ESD performance, PTFE for wear resistance. Will be LCF1010A- Features: Lubricated, Flame Retardant, Good Wear Resistance, High Flow
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names instituted after the SABIC purchase. |