MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chesterton ARC 5 Paste grade Rapid Cure Abrasion Control
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: ARC 5 is an advanced composite formulated for emergency repair and patching of metal components subject to light abrasive and corrosive conditions. It can be used to seal leaks and patch holes as well as rebuild worn surfaces quickly, returning the damaged component back to service faster than conventional welding. ARC 5 is designed to cure underwater. It is normally applied at a thickness of 3 mm (1/8”) or more. ARC 5 is 100% solids, non-shrinking.

Benefits:

  • Exceptional resistance to permeation in water immersion
  • Excellent leak repair compound due to high build characteristics in single coat application with rapid cure
  • Cures underwater
  • Tough resin structure resists thermal-mechanical shock
  • Outstanding adhesion insures reliable performance
  • Labor and downtime are reduced due to ease of application and rapid curing
  • Convenient 4-1 mix ratio and verification of mix by color change
  • Cures at temperatures as low as 4°C(40°F)

Suggested Uses:

  • Condensers
  • Cooling Water Pumps
  • Flange Faces
  • Pump Volutes
  • Valve Bodies
  • Pneumatic Transport Lines
  • Pipe Elbows
  • Pitted Pipes
  • Heat Exchangers
  • Pitted Tanks and Vessels

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³Cured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ASTM D2240
Tensile Strength at Break 17.8 MPa2580 psiASTM D638
Flexural Strength 26.9 MPa3900 psiASTM D790
Flexural Modulus 2.90 GPa420 ksiASTM D790
Compressive Strength 62.1 MPa9000 psiASTM D790
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 66.0 °C151 °FWet Service
 93.0 °C199 °FDry Service
 
Processing PropertiesMetricEnglishComments
Cure Time  15.0 min
@Temperature 32.0 °C
0.250 hour
@Temperature 89.6 °F
Light Load
 19.8 min
@Temperature 25.0 °C
0.330 hour
@Temperature 77.0 °F
Light Load
 25.00 min
@Temperature 32.0 °C
0.4167 hour
@Temperature 89.6 °F
Full Load
 35.0 min
@Temperature 16.0 °C
0.583 hour
@Temperature 60.8 °F
Light Load
 45.0 min
@Temperature 25.0 °C
0.750 hour
@Temperature 77.0 °F
Full Load
 49.8 min
@Temperature 4.00 °C
0.830 hour
@Temperature 39.2 °F
Light Load
 60.0 min
@Temperature 16.0 °C
1.00 hour
@Temperature 60.8 °F
Full Load
 60.0 min
@Temperature 32.0 °C
1.00 hour
@Temperature 89.6 °F
Full Chemical
 75.0 min
@Temperature 4.00 °C
1.25 hour
@Temperature 39.2 °F
Full Load
 120 min
@Temperature 25.0 °C
2.00 hour
@Temperature 77.0 °F
Full Chemical
 180 min
@Temperature 16.0 °C
3.00 hour
@Temperature 60.8 °F
Full Chemical
 480 min
@Temperature 4.00 °C
8.00 hour
@Temperature 39.2 °F
Full Chemical
Tack-Free Time  7.002 min
@Temperature 32.0 °C
0.1167 hour
@Temperature 89.6 °F
 10.0 min
@Temperature 25.0 °C
0.167 hour
@Temperature 77.0 °F
 19.8 min
@Temperature 16.0 °C
0.330 hour
@Temperature 60.8 °F
 30.0 min
@Temperature 4.00 °C
0.500 hour
@Temperature 39.2 °F
 
Descriptive Properties
ColorMedium Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPTCHS044 / 138156

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.