MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Tipco Tipcolite® THD 311 Phenolic Compound, Wood Flour, having Medium Flow & High Strength
Categories: Polymer; Thermoset; Phenolic

Material Notes: Medium Flow Phenolic Compound, Reinforced with Wood Flour

Applications: Electrical & Electronics

Processing: Compression Molding

Information provided by the Manufacturer, Tipco Industries Ltd., India.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.36 g/ccASTM D792
Apparent Bulk Density 0.620 g/ccTRM-37
Linear Mold Shrinkage 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 50.0 MPaASTM D638
Flexural Yield Strength 82.0 MPaASTM D790
Izod Impact, Unnotched (ISO) 2.20 kJ/m²ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmASTM D257
Surface Resistance 1.00e+10 ohmASTM D257
Dielectric Strength 9.50 kV/mmASTM D149

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tipco Tipcolite® TX 211 Phenolic Compound, Wood Flour, having Medium Flow & High Electrical Properties
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength
RTP Company RTP 199 X 130883 A Polypropylene (PP), Glass Fiber - Cellulose Fiber - 20% Renewable Resource Content
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded
RTP Company RTP 199 X 132474 A Polypropylene (PP), Copolymer - Cellulose Fiber - 20% Renewable Resource Content

PTIP1020 / 70258

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.