Product Description: Eastman™ Ethylene Glycol Diacetate (EGDA) is a colorless, low odor, very slow-evaporating solvent that gives good flow-out to baking lacquers and enamels. Its major uses are in thermoplastic acrylic coatings as a reflow solvent and in foundry core-binding applications. Application/Uses: - Coatings - Automotive OEM
- Coatings - Transportation
- Foundry Core - Binding Resins
- Graphic Arts - Screen Inks
Key Attributes:- High blush resistance
- Low MIR value
- Non-HAP
- Non-SARA
- Predicted to be readily biodegradable
- Slow evaporation rate
Information provided by Eastman |