Hostacom TYS1365NC NH533 BLK is a high melt flow, unfilled, UV stabilized, flexible olefin compound. The product has been developed for industrial and automotive applications where a combination of good processability and excellent softness is required. This grade is available in black, pellet form. Applications: Automotive Parts, IndustrialInformation provided by LyondellBasell. |