MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Westlake MXSTEN® CV77525 LLDPE Plastomer
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Extrusion Grade

Material Notes: MXSTEN® CV77525 is a linear low density polyethylene plastomer with very low levels of antioxidants. It does not contain any slip or antiblock additives. It is recommended as a core layer to increase the dart impact, puncture resistance, and tear properties for multilayer films that are post electron beam treated.

Test specimens for blown film: nominal thickness 1.0 mils; blow up ratio 2.5:1, die gap 100 mils at 50% relative humidity and 23°C.

Information provided by Westlake Chemical.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.906 g/cc0.0327 lb/in³ASTM D4883
Melt Index of Compound 0.50 g/10 min0.50 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 700 %700 %ASTM D882
Film Elongation at Break, TD 950 %950 %ASTM D882
Elmendorf Tear Strength, MD 17.7 g/micron450 g/milASTM D1922
Elmendorf Tear Strength, TD 29.5 g/micron750 g/milASTM D1922
Dart Drop 68.9 g/micron1750 g/milASTM D1709
Film Tensile Strength at Break, MD 55.2 MPa8010 psiASTM D882
Film Tensile Strength at Break, TD 44.8 MPa6500 psiASTM D882
1% Secant Modulus, MD 110 MPa16000 psiASTM D882
1% Secant Modulus, TD 96.5 MPa14000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 14 %14 %ASTM D1003
Gloss 55 %55 %@ 45°; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 216 - 232 °C420 - 450 °FWith blow-up ratios of 1.5:1 or higher.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8723 / 287833

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.