MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vinnolit® S 3250/13 Vinyl Chloride/Vinyl Acetate Copolymer Suspension
Categories: Polymer; Thermoplastic; Vinyl (PVC); Polyvinyl Chloride - Polyvinyl Acetate Copolymer

Material Notes: Vinnolit® S 3250/13 Suspension copolymer of vinyl chloride and vinyl acetate for thermoplastic processing. Vinnolit® S 3250/13 is a free-flowing powder produced by suspension copolymerization of vinyl chloride and vinyl acetate. The product contains about 13 percent vinyl acetate. It is a specialty resin for vinyl records, rigid or semi-rigid films and flooring applications (e. g. LVT). Blends containing with Vinnolit® S 3250/13 are used to produce high quality vinyl records and calendered films/sheets e.g. for flooring constructions. The low K-value and the high acetate content provide a very good flow and processing behavior. Due to the high acetate content formulations with Vinnolit® S 3250/13 can accept very high filler loads, show fast gelling or gelling at low temperatures and provide a very good printability.

Information provided by Vinnolit.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Volatiles <= 0.50 %ISO 1269
Apparent Bulk Density 0.650 g/ccISO 60
Particle Size 63 µm>= 60% Retained on 0.063 mm Sieve; ISO 4610
 <= 250 µm<= 1% Retained on 0.25 mm Sieve; ISO 4610
Viscosity Test 0.60 dl/gReduced Viscosity; ISO 1628-2
Vinyl Acetate Content 13 %Vinnolit
 
Descriptive Properties
K-Value50ISO 1628-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVINNO919 / 291116

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.