EUROPLEX® Film HC 99710 is a highly transparent, very efficient weather and UV protection film with excellent surface properties such as chemical resistance, anti-graffiti and dirt-repellent behavior. EUROPLEX® Film HC 99710 is based on a special polymethyl methacrylate (PMMA) formulation with weather resistance, extremely high UV absorption as well as superior printability and lamination performance. It owes these surface properties to the polyvinylidene fluoride (PVDF) layer which is fused to the PMMA substrate. Information provided by Cyro Industries Information Provided by Evonik CYRO. The former Evonik Methacrylates business has been sold to Röhm GmbH, although this trade name was disontinued prior to the sale. |