MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Sibur APP-B Atactic Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: For preparation of polymer, bitumen-polymer and polymer-mineral mastics. Individual melts and compositions used for anti-corrosion covers for underground piping, different building structures, structures of industrial equipment, for improvement of mechanical-physical properties of asphalt covering and putty, as well as rubber shoe industry as additions to rubber mixtures.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement <= 500000
@Temperature 180 °C
units unknown
Collected Volatile Condensable Material <= 3.0 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 100 - 160 °C
 
Descriptive Properties
Mass Share of Isotactic Fraction<40%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sibur APP-G Atactic Polypropylene
Hong Kun Group APP (Phase II) Flame Retardant
Total PPR LX5 02-15 Polypropylene, Metallocene Film Resin
Lushan M-10H Adhesive Resin for Multi-layer Sausage Casing film
Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film

PSIB029 / 67592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.