MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Techmer ES Luriblend® PA6/6 CF30 TL15 HS BK 30% Carbon Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Carbon Fiber/PTFE Filled; Nylon 66, Heat Stabilized

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Carbon Fiber, 30% Filler by Weight

Additive: PTFE Lubricant(15%) and Heat Stabilizer

Features: Lubricated, Good Wear Resistance, Heat Stabilized and Low Friction

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.38 g/ccASTM D792
Water Absorption 0.48 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 in/in
@Thickness 3.17 mm
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ASTM D785
Tensile Strength, Yield 28000 psiASTM D638
Elongation at Break 2.5 %ASTM D638
Flexural Strength 41500 psiASTM D790
Flexural Modulus 1.98e+6 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/in
@Thickness 3.17 mm
ASTM D256
Coefficient of Friction, Dynamic 0.10ASTM D1894
Coefficient of Friction, Static 0.090ASTM D1894
K (wear) Factor 8.00 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 22000 psi-ft/min1000 fpm
 30000 psi-ft/min10 fpm
 44000 psi-ft/min100 fpm
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 10 - 10000 ohm-cmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 10.0 µin/in-°FASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 498 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 488 °FUnannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled
Cast Nylons Nycast® Nyloil® Lubricated Nylon
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6
Techmer ES Luriblend® PA6/6 CF33 ML2 BK 33% Carbon Filled
Techmer ES Luriblend® PA6 CF30 TS15 BK 30% Carbon Filled

PTPC0812 / 136750

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.