MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Avient Nymax™ 600 A Natural Polyamide 6 Alloy (Nylon 6 Alloy)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials have been formulated to provide improved melt processing, part performance, or surface appearance depending upon grade selected and are offered as an economical alternative to fully compounded products.

Molded Test Bars: Dry as Molded

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D792
Water Absorption 1.6 %
@Thickness 3.18 mm
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.012 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 77.9 MPaType I, 5.1 mm/min; ASTM D638
Elongation at Break 80 %Type I, 5.1 mm/min; ASTM D638
Flexural Strength 103 MPaASTM D790
Flexural Modulus 2690 MPaASTM D790
Izod Impact, Notched 64.0 J/m
@Thickness 3.18 mm,
Temperature 23.0 °C
Injection Molded; ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 215 °CASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 150 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °C
@Thickness 3.18 mm
Unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Mold Temperature 48.9 - 93.3 °C
Drying Temperature 82.2 °C
Dry Time 4.00 hour
 
Descriptive Properties
AppearanceNatural Color
FeaturesGeneral Purpose
FormsPellets
Generic MaterialNylon 6 Alloy
Generic NamePolyamide 6 Alloy (Nylon 6 Alloy)
Processing MethodInjection Molding
Regional AvailabilityNorth America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Nymax™ 600 A HS Natural A Polyamide 6 Alloy (Nylon 6 Alloy)
Avient Nymax™ 600 A Natural 12 Polyamide 6 Alloy (Nylon 6 Alloy)
Avient Nymax™ 600 Zip 0 Black 13 Polyamide 6 Alloy (Nylon 6 Alloy)

PH0POL0022 / 144591

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.