MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY 8000-05 Polycarbonate, Injection Molded
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: Introduction: LUPOY PC 8000-05 polycarbonate (PC) siloxane copolymer resin is designed for extrusion and injection molding products. It exhibits an excellent low temperature ductility and good physical property balance of heat resistance, transparency and impact strength.

Main Characteristics: Low Temperature ductility, No UV absorbers, No Mold release agent

Applications: Compounds, Small appliances, Packaging applications

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.12 %
@Time 86400 sec
0.12 %
@Time 24.0 hour
ASTM D570
Moisture Absorption at Equilibrium 0.20 %0.20 %50% RH; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Melt Flow 3.3 g/10 min
@Load 1.20 kg,
Temperature 300 °C
3.3 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 5050ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Ultimate 68.0 MPa9860 psiASTM D638
Tensile Strength, Yield 58.0 MPa8410 psi50mm/min; ASTM D638
Elongation at Break 120 %120 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.18 GPa316 ksiASTM D638
Flexural Strength 86.0 MPa12500 psiASTM D790
Flexural Modulus 2.03 GPa294 ksiASTM D790
Izod Impact, Notched  7.47 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
14.0 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
0.25 mm notch; ASTM D256
 9.07 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
17.0 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
0.25 mm notch; ASTM D256
Izod Impact, Unnotched NBNBASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmdry; ASTM D 257
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature -40.0 - 82.0 °C
38.9 µin/in-°F
@Temperature -40.0 - 180 °F
ASTM D 696
Deflection Temperature at 0.46 MPa (66 psi) 132 °C
@Thickness 3.20 mm
270 °F
@Thickness 0.126 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)  118 °C
@Thickness 3.20 mm
244 °F
@Thickness 0.126 in
Unannealed; ASTM D648
 130 °C
@Thickness 3.20 mm
266 °F
@Thickness 0.126 in
Annealed; ASTM D648
Vicat Softening Point 138 °C
@Load 5.00 kg
280 °F
@Load 11.0 lb
50°C/h; ASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze <= 1.0 %<= 1.0 %ASTM D1003
Transmission, Visible >= 88 %>= 88 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLHCHEM9729 / 239253

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.