MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Latrobe LSS™ A7 Mod. Wear-Resistant Tool Steel (ASTM A7 Mod.)
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel; Tool Steel

Material Notes: TLS A7 Mod. is a chromium-modified A7 type air-hardening tool steel that exhibits exceptional wear resistance. The high carbon and vanadium contents result in numerous, hard vanadium carbide particles in the steel. These carbides exhibit a hardness that is equivalent to approximately 80 to 85 Rockwell C. TLS A7 Mod. tool steel resists wear from sliding contact with other steels as well as from contact with dry and wet slurries of hard abrasive particles such as sand, shot blast media, and ceramics. Typical applications include brick mold liners, sand slinger liners, shot blasting equipment liners, extrusion tools for ceramics, powder compaction tooling, and machine tool ways.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.66 g/cc0.277 lb/in³literature value
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell C 6767Air Cooled from 927°C, 30 minutes
 6868Air Cooled from 982°C, 30 minutes
Machinability 20 - 25 %20 - 25 %1% Carbon Steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 2.6 %2.6 %
Chromium, Cr 8.25 %8.25 %
Iron, Fe 82.545 %82.545 %
Manganese, Mn 0.60 %0.60 %
Molybdenum, Mo 1.2 %1.2 %
Silicon, Si 0.30 %0.30 %
Sulfur, S <= 0.0050 %<= 0.0050 %
Vanadium, V 4.5 %4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI Type D2 Tool Steel, air-quenched from 1010°C, tempered at 315°C
AISI Type P20 Mold Steel (UNS T51620)
AISI Type P2 Mold Steel (UNS T51602)
Latrobe BR-3® High Carbon-Medium Chromium Die Steel (AISI A7)
AISI Type P4 Mold Steel, air cooled from 955°C, tempered at 425°C

NTIMK102 / 19449

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.