MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Overview of materials for Alpha/Near Alpha Titanium Alloy
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Near Alpha Titanium Alloy

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Alpha/Near Alpha Titanium Alloy". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 4.31 - 4.84 g/ccAverage value: 4.50 g/cc Grade Count:55
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 256 - 334Average value: 305 Grade Count:18
Hardness, Knoop 278 - 363Average value: 333 Grade Count:18
Hardness, Rockwell C 15.0 - 36.0Average value: 30.7 Grade Count:23
Hardness, Vickers 269 - 350Average value: 320 Grade Count:21
Tensile Strength, Ultimate 620 - 1180 MPaAverage value: 883 MPa Grade Count:54
Tensile Strength, Yield 480 - 1070 MPaAverage value: 778 MPa Grade Count:55
Elongation at Break 3.00 - 25.0 %Average value: 13.4 % Grade Count:54
Reduction of Area 13.0 - 47.0 %Average value: 27.8 % Grade Count:30
Modulus of Elasticity 91.0 - 125 GPaAverage value: 114 GPa Grade Count:48
Compressive Yield Strength 690 - 1080 MPaAverage value: 881 MPa Grade Count:8
Compressive Modulus 118 - 130 GPaAverage value: 124 GPa Grade Count:5
Notched Tensile Strength 790 - 1650 MPaAverage value: 1220 MPa Grade Count:10
Ultimate Bearing Strength 1760 - 2000 MPaAverage value: 1890 MPa Grade Count:4
Bearing Yield Strength 1340 - 1620 MPaAverage value: 1470 MPa Grade Count:4
Poissons Ratio 0.300 - 0.330Average value: 0.311 Grade Count:36
Fatigue Strength 110 - 1000 MPaAverage value: 431 MPa Grade Count:25
Fracture Toughness 33.0 - 910 MPa-m½Average value: 143 MPa-m½ Grade Count:18
Shear Modulus 24.0 - 48.2 GPaAverage value: 44.1 GPa Grade Count:36
Shear Strength 520 - 690 MPaAverage value: 608 MPa Grade Count:6
Charpy Impact 15.0 - 92.0 JAverage value: 40.7 J Grade Count:20
Bend Radius, Minimum 2.00 - 6.00 tAverage value: 4.00 t Grade Count:17
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000650 - 0.000198 ohm-cmAverage value: 0.000152 ohm-cm Grade Count:42
 
Thermal PropertiesOriginal ValueComments
CTE, linear 7.70 - 11.3 µm/m-°CAverage value: 9.35 µm/m-°C Grade Count:45
Specific Heat Capacity 0.460 - 0.552 J/g-°CAverage value: 0.519 J/g-°C Grade Count:34
Thermal Conductivity 4.15 - 13.0 W/m-KAverage value: 7.64 W/m-K Grade Count:46
Melting Point 1540 - 1710 °CAverage value: 1650 °C Grade Count:31
Solidus 1700 °CAverage value: 1700 °C Grade Count:4
Liquidus 1540 - 1710 °CAverage value: 1640 °C Grade Count:29
Maximum Service Temperature, Air 350 - 760 °CAverage value: 511 °C Grade Count:15
Beta Transus 895 - 1110 °CAverage value: 998 °C Grade Count:46
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 2.25 - 8.35 %Average value: 5.23 % Grade Count:53
Carbon, C 0.0300 - 0.400 %Average value: 0.0730 % Grade Count:46
Copper, Cu 2.00 - 3.00 %Average value: 2.50 % Grade Count:4
Hydrogen, H 0.00600 - 0.100 %Average value: 0.0212 % Grade Count:43
Iron, Fe 0.0300 - 0.500 %Average value: 0.208 % Grade Count:46
Molybdenum, Mo 0.200 - 2.20 %Average value: 0.996 % Grade Count:35
Niobium, Nb (Columbium, Cb) 0.500 - 2.00 %Average value: 1.54 % Grade Count:10
Nitrogen, N 0.0100 - 0.400 %Average value: 0.0413 % Grade Count:47
Oxygen, O 0.0200 - 0.200 %Average value: 0.135 % Grade Count:47
Palladium, Pd 0.0400 - 0.0800 %Average value: 0.0567 % Grade Count:3
Silicon, Si 0.0150 - 0.600 %Average value: 0.253 % Grade Count:17
Tantalum, Ta 1.00 %Average value: 1.00 % Grade Count:6
Tin, Sn 0.600 - 11.0 %Average value: 3.51 % Grade Count:19
Titanium, Ti 81.0 - 98.0 %Average value: 90.4 % Grade Count:57
Vanadium, V 0.600 - 3.00 %Average value: 1.91 % Grade Count:25
Zirconium, Zr 0.600 - 6.00 %Average value: 3.59 % Grade Count:20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Alpha/Beta Titanium Alloy
Overview of materials for Beta Titanium Alloy
Overview of materials for Unalloyed/Modified Titanium
Titanium Alloys, General
Titanium, Ti

M01071 / 81699

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.