MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® F 50 nat 6368 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product description: Grilon F 50 natural 6368 is a modified, very high viscous Polyamide 6 for extrusion processes:
  • Very high melt strength
  • Good chemical resistance
  • Good gas-barrier
  • Good mechanical properties
  • Good barrier against oil & fat
  • Improved processing and slip properties
Application examples: Grilon F 50 natural 6368 is used for pipe extrusion, extrusion blown containers and various semi-finished products, where high melt strength is required. It can also be used for Sliding rails, in-liner for cans, sheets etc.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccDry; ISO 1183
Water Absorption 9.0 %Sim. to ISO 62
Moisture Absorption 3.00 %Sim. to ISO 62
Water Vapor Transmission 15.0 g/m²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 45 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 35.0 MPaISO 527-3
Film Tensile Strength at Yield, TD 30.0 MPaISO 527-3
Film Elongation at Break, MD 700 %ISO 527-3
Film Elongation at Break, TD 700 %ISO 527-3
Film Elongation at Yield, MD 15 %ISO 527-3
Film Elongation at Yield, TD 15 %ISO 527-3
Tensile Modulus 750 MPaConditioned; ISO 527-1/-2
 3000 MPaDry; ISO 527-1/-2
Charpy Impact, Notched 5.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 6.00 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
Tear Strength 30.0 kN/mTrouser Tear Resistance, Parallel; ISO 6383-1
 30.0 kN/mTrouser Tear Resistance, Normal; ISO 6383-1
Film Tensile Strength at Break, MD 100 MPaISO 527-3
Film Tensile Strength at Break, TD 90.0 MPaISO 527-3
 
Thermal PropertiesOriginal ValueComments
Melting Point 222 °C10°C/min; ISO 11357-1/-3
 
Optical PropertiesOriginal ValueComments
Gloss 100 %60°; ISO 2813
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)250ISO 15105-1/-2; 23°C/ 85% RH
 80ISO 15105-1/-2; 23°C/0% RH
Elmendorf Tear Resistance, Normal (N)10ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)10ISO 6383-2
EMS Gelboflextest [holes/m²]900
Food contactEU Requirements
FormGranules
Gelboflextest [holes/m²], EMS900
Industry & Consumer goodsMechanical Engineering
Oxygen Transmission Rate, cm³/(m²*d*bar)25ISO 15105-1/-2; 23°C/0% RH
 50ISO 15105-1/-2; 23°C/ 85% RH
PackagingBlow molded containers
 Injection, stretch, blow molded containers
ProcessingBlown Film Extrusion
 Extrusion - blow molding
 Other Extrusion
Product AttributesBarrier Properties
 High viscosity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilon® F 34 NL PA6
Envalior Akulon® F136 PA6, Very High Viscosity, Film Extrusion
EMS-Grivory Grilon® FG 34 NL nat 6023 PA6
EMS-Grivory Grilon® F 47 NL nat 6028 PA6
EMS-Grivory Grilon® BG-30 S FA PA6-GF30

PGRH241 / 156950

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.